Electrically conductive liquid silicone rubber. ELASTOSIL® LR 3162 A/B is a paste-like, two component compound with short curing times. Properties: The vulcanizates are noted for good mechanical as well as electrical properties and for good heat resistance within a temperature range of -55°C to+210°C. Information provided by Wacker Chemie AG. |