MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 3162 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Electrically conductive liquid silicone rubber. ELASTOSIL® LR 3162 A/B is a paste-like, two component compound with short curing times.

Properties: The vulcanizates are noted for good mechanical as well as electrical properties and for good heat resistance within a temperature range of -55°C to+210°C.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183-1 A
Viscosity 6.60e+6 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53DIN 53505
Tensile Strength at Break 5.50 MPaDIN 53504 S 1
Elongation at Break 400 %DIN 53504 S 1
Rebound 54 %DIN 53512
Tear Strength 18.0 kN/mASTM 624 B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 11 ohm-cmDIN VDE 0303
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °C
Minimum Service Temperature, Air -55.0 °C
Flammability, UL94 HB
@Thickness 0.500 - 0.800 mm
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Treatment Temp. 165 °C
in press
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 35 %EN ISO 4589-2/ASTM D2863
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon 30600R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Momentive Performance Materials Silopren™ LSR 2670 Liquid Silicone Rubber - Fast Cure / High Tear
Momentive Performance Materials Silopren™ LIM 6061 Liquid Silicone Rubber - Fast Cure / High Tear

PWACK9149 / 204678

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.