MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ceradyne Ceralloy® 546-3E Boron Carbide  (discontinued **)
Categories: Ceramic; Carbide

Material Notes:

Features:

  • low porosity
  • high purity
  • single phase
  • Applications:

  • semiconductor components
  • Information provided by Ceradyne Company

    Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 2.50 g/cc
    Grain Size 15 µm
    Weibull Modulus 12
     
    Mechanical PropertiesOriginal ValueComments
    Vickers Microhardness 2800
    Modulus of Elasticity 460 GPa
    Flexural Strength 410 MPa
    @Temperature 23.0 °C
    Poissons Ratio 0.17
    Fracture Toughness 2.50 MPa-m½
    Shear Modulus 197 GPacalculated
     
    Electrical PropertiesOriginal ValueComments
    Electrical Resistivity 10.0 ohm-cm
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 5.60 µm/m-°C
    @Temperature 20.0 - 1000 °C
    Thermal Conductivity 90.0 W/m-K
     
    Descriptive Properties
    Purity, %98.5

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Ceradyne Ceralloy® 546 Boron Carbide
    Boron Carbide, B4C
    3M Techical Ceramics Boron Carbide Powder
    Ceradyne Ceralloy® 546-4E Boron Carbide
    CoorsTek RB B4C Reaction-Bonded Boron Carbide

    CCERDN12 / 695

    New MatWeb Services

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.