MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Techical Ceramics Boron Carbide Powder
Categories: Ceramic; Carbide

Material Notes: Know as TETRABOR® when a ESK Ceramics product.

Information provided by 3M Technical Ceramics, formerly ESK Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 2.48 g/cc>= 0.0896 lb/in³DIN EN 623-2
Porosity <= 0.50 %<= 0.50 %DIN EN 623-2
 <= 1.0 %<= 1.0 %DIN EN 623-2
Grain Size <= 10 µm<= 10 µm
Weibull Modulus 1515[m]; DIN EN 843-5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 27
@Pressure 100 MPa
27
@Pressure 14500 psi
DIN EN 843-4
Hardness, Vickers  26
@Pressure 1000 MPa
26
@Pressure 145000 psi
DIN EN 843-4
 31
@Pressure 50.0 MPa
31
@Pressure 7250 psi
DIN EN 843-4
Tensile Modulus 420 GPa60900 ksiYoung's; DIN EN 843-2
Flexural Strength 460 MPa66700 psi4-pt bending; DIN EN 843-1
Compressive Strength >= 2800 MPa>= 406000 psiDIN 51104
Poissons Ratio 0.180.18DIN EN 843-2
Fracture Toughness 5.00 MPa-m½4.55 ksi-in½SENB
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00 ohm-cm1.00 ohm-cmDIN EN 50359
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.50 µm/m-°C
@Temperature 25.0 - 500 °C
2.50 µin/in-°F
@Temperature 77.0 - 932 °F
DIN EN 821-1
 6.30 µm/m-°C
@Temperature 500 - 1000 °C
3.50 µin/in-°F
@Temperature 932 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.940 J/g-°C0.225 BTU/lb-°FC DIN EN 821-3
Thermal Conductivity 36.0 W/m-K250 BTU-in/hr-ft²-°FDIN EN 821-2
 
Descriptive Properties
ColorSilver gray metallic
Microstructurefine-grained
Sonic velocity13500 m/sDIN EN 843-2
Thermal Stress204 KR1 = sB·(1-ν)/(α·E)
 7 W/mmR2= R1-λ

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 546-3E Boron Carbide
Silicon Carbide, CVD
Ceradyne Ceralloy® 546 Boron Carbide
CeramTec CD 110 Silicon Carbide, SSiC
CoorsTek RB B4C Reaction-Bonded Boron Carbide

CESK04 / 183296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.