Features: Excellent clarity, blush resistant and good flexural modulus. Product does not contain animal derived components. Applications: Injection Molded - Lab ware, food packaging and medical. Suitable for autoclave sterilization processes in the presences of aqueous solutions. Information provided by Flint Hills Resources. |