MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Flint Hills 11R12A Specialty Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Features: Good drop impact, radiation resistant. Product does not contain animal derived components and is phthalate-free.

Applications: Injection Molding

Information provided by Flint Hills Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 12 g/10 min12 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 29.5 MPa4280 psiASTM D638
Elongation at Yield 9.0 %9.0 %ASTM D638
Flexural Modulus 0.942 GPa137 ksiTangent; ASTM D790
Izod Impact, Notched 0.370 J/cm0.693 ft-lb/inASTM D256
Gardner Impact 35.5 J26.2 ft-lbASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1520(c) 1.1a and 3.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills P9M7R-056 Specialty Homopolymer Polypropylene
Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer
Flint Hills 13T25A Random Copolymer Polypropylene
Flint Hills AP7535-HS Polypropylene Ultra High Impact Copolymer
Flint Hills P4G4K-038 Homopolymer Polypropylene

PFLINT804 / 142616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.