MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI 1018 Steel, hot rolled, quenched, and tempered
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Medium low-carbon steel, has good weldability and slightly better machinability than lower carbon grades.

Key Words: carbon steel, AMS 5069, ASTM A108, UNS G10180, AS 1442 K1018 (Australia), AS 1443 K1018, CSN 12020 (Czech), CSN 12022, AFNOR NF A33-101 AF42C20, DIN 1.0453, DIN C16.8, DGN B-301 1018 (Mexico), COPANT 331 1018 (Pan America), COPANT 333 1018, MST.T (Russia), ST.20A, ST.3, ST.3T, GOST M18S, GOST 23570 18ps, GOST 23570 18sp, GOST 5520 18K, GOST 5521 S, NBN 629 D37-2 (Belgium), NBN 630 E37-1, NBN 630 E37-2, NBN A21-221 C17KD, BDS 9801 S (Bulgaria), GB 715 ML3 (China), TS 302 Fe35.2 (Turkey), TS 346 Fe35, BS 970 080A17, DEF STAN95-1-1 C1018
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 143
Hardness, Knoop 163Converted from Brinell
Hardness, Rockwell B 78Converted from Brinell
Hardness, Vickers 149Converted from Brinell
Tensile Strength, Ultimate 475 MPa
Tensile Strength, Yield 275 MPa
Elongation at Break 38 %In 50 mm
Reduction of Area 62 %
Modulus of Elasticity 200 GPa
Bulk Modulus 159 GPaEstimated from elastic modulus
Poissons Ratio 0.29Typical for steel
Machinability 52 %Based on AISI 1212 steel = 100%
Shear Modulus 78.0 GPaEstimated from elastic modulus
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000159 ohm-cm
@Temperature 0.000 °C
annealed condition
 0.0000219 ohm-cm
@Temperature 100 °C
annealed condition
 0.0000293 ohm-cm
@Temperature 200 °C
annealed condition
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.486 J/g-°C
@Temperature >=100 °C
annealed
Thermal Conductivity 49.8 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.14 - 0.20 %
Iron, Fe 98.81 - 99.26 %As remainder
Manganese, Mn 0.60 - 0.90 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1018 Steel, cold drawn, quenched, and tempered, 19-32 mm (0.75-1.25 in) round
ASTM A36 Steel, plate
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round

M1018B / 6810

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.