MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9555 Adhesive Transfer Tapes with Adhesive 220
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 124 microns4.90 mil
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.438 kN/m2.50 pliStainless Steel, 90° peel, 2 mil aluminum foil backing, 15 min at RT, 2.3 mil; ASTM D3330
 0.58068 kN/m3.3125 pliStainless Steel, 90° peel, 2 mil aluminum foil backing, 15 min at RT, 4.9 mil; ASTM D3330
 0.60259 kN/m3.4375 pliABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
 0.60259 kN/m3.4375 plipolycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
 0.69024 kN/m3.9375 plipolycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
 0.71216 kN/m4.0625 pliABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
 0.7669 kN/m4.375 pliglass, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
 0.8108 kN/m4.625 pliStainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
 0.97511 kN/m5.5625 pliglass, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
 1.074 kN/m6.125 pliStainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
 1.4353 kN/m8.1875 pliStainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 2.3 mil; ASTM D3330
 1.895 kN/m10.81 pliStainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 4.9 mil; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FLong term
 177 °C351 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Adhesive Type220
LinerTan 58# Polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP-100 Epoxy Adhesive
3M Scotchkote™ HTX 517 Epoxy HT Lining
Overview of materials for High Density Polyethylene (HDPE), Extruded
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
3M Scotch-Weld™ DP 3501 Epoxy Adhesive

PMM33242 / 167989

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.