MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ DP-100 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 8000 - 15000 cP8000 - 15000 cPBase, RVF #6 spindle, 20 rpm @ 27°C
 9000 - 16000 cP9000 - 16000 cPAccelerator, RVF #6 spindle, 20 rpm @ 27°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8580 - 85ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.50e+12 ohm-cm3.50e+12 ohm-cmASTM D257
Dielectric Strength 33.9 kV/mm860 kV/inASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear  60.0 µm/m-°C
@Temperature -40.0 - 20.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 68.0 °F
 209 µm/m-°C
@Temperature 60.0 - 120 °C
116 µin/in-°F
@Temperature 140 - 248 °F
Thermal Conductivity 0.184 W/m-K
@Temperature 45.0 °C
1.28 BTU-in/hr-ft²-°F
@Temperature 113 °F
Glass Transition Temp, Tg 33.0 °C91.4 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 - 2880 min24.0 - 48.0 hour
 
Descriptive Properties
AppearanceClear/Light Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
3M Scotchkote™ HTX 517 Epoxy HT Lining
Overview of materials for High Density Polyethylene (HDPE), Extruded
3M GM110 Gripping Material
3M 9555 Adhesive Transfer Tapes with Adhesive 220

PMM34614 / 169361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.