MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives 6100 Silver Conductor
Categories: Polymer; Thermoset; Epoxy

Material Notes: LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and discrete component surface mount applications.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 100000 - 150000 cP
@Temperature 25.0 °C
100000 - 150000 cP
@Temperature 77.0 °F
RVT, Spindle #7 @ 20rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 55.2 - 68.9 MPa8000 - 10000 psiDie; Bare Si die on alumina
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.050 ohm<= 0.050 ohm
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 - 60.0 min
@Temperature 150 °C
0.500 - 1.00 hour
@Temperature 302 °F
 
Descriptive Properties
AppearanceSilver
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay VTM® 260 series Epoxy Resin
Solvay METLBOND® 1515-4 Epoxy Film Adhesive
Armstrong X-81-A/F Epoxy Adhesive
Armstrong X-81/A Epoxy Adhesive
Armstrong C-1/A Epoxy Adhesive

PLORD050 / 86058

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.