MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Versalis Sinkral® B 532/E ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded sheet. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-25-20

Applications: Large sheets with good surface finish (co-extruded or not and suitable for high draw ratios) for a variety of uses in sectors such as refrigeration, sanitary, automotive, packaging and furniture (profiles).

Grade available in natural color only. Suitable masterbatches could be recommended for self-coloring.

Information provided by Polimeri Europa

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption 0.30 %0.30 %24 hours - 23°C; ASTM D 570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/in
Melt Flow 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ISO 2039/2
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ASTM D 638
Elongation at Break 45 %45 %50 mm/min; ASTM D 638
Flexural Strength 68.0 MPa9860 psi2 mm/min; ASTM D 790
Flexural Modulus 2.30 GPa334 ksi2 mm/min; ASTM D 790
Izod Impact, Notched  1.25 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
2.34 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ISO 180/4A
 1.50 J/cm
@Thickness 3.20 mm,
Temperature -20.0 °C
2.81 ft-lb/in
@Thickness 0.126 in,
Temperature -4.00 °F
ISO 180/4A
 1.90 J/cm
@Thickness 3.20 mm,
Temperature 0.000 °C
3.56 ft-lb/in
@Thickness 0.126 in,
Temperature 32.0 °F
ISO 180/4A
 2.80 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
5.25 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ISO 180/4A
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Thickness 4.00 mm,
Temperature -40.0 °C
4.76 ft-lb/in²
@Thickness 0.157 in,
Temperature -40.0 °F
ISO 180/1A
 20.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
9.52 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DIN 53453
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmDry; IEC 60093
Dielectric Constant 3.1
@Frequency 1000 Hz
3.1
@Frequency 1000 Hz
Dry; IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inDry; IEC 60243
Dissipation Factor 0.015
@Frequency 1000 Hz
0.015
@Frequency 1000 Hz
dry; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
50.0 µin/in-°F
@Temperature 68.0 °F
ASTM D 696
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FASTM C 177
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °F120°C/h; ASTM D 648
Vicat Softening Point 104 °C219 °F50 N - 120°C/h; ISO 306/B120
 108 °C226 °F10 N - 120°C/h; ISO 306/A120
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Glow Wire Test 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
IEC 60695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Drying Temperature 80.0 °C176 °FNo venting in an air circulating oven
Dry Time 2 - 4 hour2 - 4 hourNo venting in an air circulating oven

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess MACROLEX® Blue RR Blue Pigment
INEOS Styrolution Terluran® HI-12 ABS
INEOS Styrolution Terluran® GP-25 ABS
INEOS Styrolution Terluran® EGP-7 ABS
Ineos ABS Lustran® 648

PENJ55 / 35930

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.