MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lanxess MACROLEX® Blue RR Blue Pigment
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Anthraquinone dyestuff

Main fields of application: Transparent and opaque dyeing of PS, SAN, PMMA, PC, ABS and ABS / PC blends.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.460 g/cc0.0166 lb/in³DIN ISO 787-11
Density 1.18 g/cc0.0426 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  22 %
@Thickness 2.00 mm,
Wavelength 635 nm
22 %
@Thickness 0.0787 in,
Wavelength 635 nm
0.01% Dyestuff
 25 %
@Thickness 2.00 mm,
Wavelength 585 nm
25 %
@Thickness 0.0787 in,
Wavelength 585 nm
0.01% Dyestuff
 30 %
@Thickness 2.00 mm,
Wavelength 605 nm
30 %
@Thickness 0.0787 in,
Wavelength 605 nm
0.01% Dyestuff
 58 %
@Thickness 2.00 mm,
Wavelength 640 nm
58 %
@Thickness 0.0787 in,
Wavelength 640 nm
0.003% Dyestuff
 60 %
@Thickness 2.00 mm,
Wavelength 585 nm
60 %
@Thickness 0.0787 in,
Wavelength 585 nm
0.003% Dyestuff
 60 %
@Thickness 2.00 mm,
Wavelength 360 nm
60 %
@Thickness 0.0787 in,
Wavelength 360 nm
0.01% Dyestuff
 65 %
@Thickness 2.00 mm,
Wavelength 605 nm
65 %
@Thickness 0.0787 in,
Wavelength 605 nm
0.003% Dyestuff
 75 %
@Thickness 2.00 mm,
Wavelength 360 nm
75 %
@Thickness 0.0787 in,
Wavelength 360 nm
0.003% Dyestuff
 84 %
@Thickness 2.00 mm,
Wavelength 460 nm
84 %
@Thickness 0.0787 in,
Wavelength 460 nm
0.01% Dyestuff
 86 %
@Thickness 2.00 mm,
Wavelength 450 nm
86 %
@Thickness 0.0787 in,
Wavelength 450 nm
0.003% Dyestuff
 90 %
@Thickness 2.00 mm,
Wavelength 700 nm
90 %
@Thickness 0.0787 in,
Wavelength 700 nm
0.003% Dyestuff
 90 %
@Thickness 2.00 mm,
Wavelength 720 nm
90 %
@Thickness 0.0787 in,
Wavelength 720 nm
0.01% Dyestuff
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month60.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess MACROLEX® Blue RR Gran Blue Pigment
Lanxess MACROLEX® Red E2G Gran Red Pigment
Lanxess MACROLEX® Red E2G Red Pigment
Lanxess MACROLEX® Red B Red Pigment
Lanxess MACROLEX® Orange R Gran Orange Pigment

PLANY8865 / 209257

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.