Homopolymer film grade Low Residuals - Fina 3374X utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity. Slip/Antiblock - Fina 3374X is available with custom slip and antiblock packages. FDA - Fina 3374X complies with all application FDA regulations for food contact applications. Recommended Applications - Fina 3374X is recommended in orientation processes for manufacture of packaging tapes and films. Processing - Fina 3374X resin processes on oriented film extrusion equipment with typical melt temperatures of 450°F-525°F (232°C-274°C). Data provided by the manufacturer, Total Petrochemicals. Total Petrochemicals includes former Fina and Atofina plastics product lines. |