MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Total 3374X Polypropylene, Oriented Film Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Homopolymer film grade

Low Residuals - Fina 3374X utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.

Slip/Antiblock - Fina 3374X is available with custom slip and antiblock packages.

FDA - Fina 3374X complies with all application FDA regulations for food contact applications.

Recommended Applications - Fina 3374X is recommended in orientation processes for manufacture of packaging tapes and films.

Processing - Fina 3374X resin processes on oriented film extrusion equipment with typical melt temperatures of 450°F-525°F (232°C-274°C).

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Permeability 4.70 g mil/ (m2 day)
@Temperature 37.8 °C
0.303 g mil/ (100 in2 day)
@Temperature 100 °F
90% RH; ASTM E96
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %ASTM D882
Film Elongation at Break, TD 50 %50 %ASTM D882
Secant Modulus, MD 1.70 GPa247 ksiASTM D882
Secant Modulus, TD 3.10 GPa450 ksiASTM D882
Film Tensile Strength at Break, MD 140 MPa20300 psiASTM D882
Film Tensile Strength at Break, TD 230 MPa33400 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %ASTM D1003
Gloss 85 %85 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 274 °C450 - 525 °Foriented film extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFIN59 / 38389

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.