MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Performance Alloys MoldStar® 150 (PAS 940) Copper Mold Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Description: MoldStar® 150 is a high-performance, beryllium-free copper alloy for the blow molding and injection molding industries. In addition to its high thermal conductivity, MoldStar® 150 offer the following qualities:
  • Accepts and maintains high surface finishes
  • Accepts etching and texturing
  • Offers welding compatibility with other copper alloys, tool steels and stainless steels to provide composite materials for increased surface hardness in specific areas
  • Requires no additional heat treatment
  • Retains the inherent corrosion resistance of copper
  • Can be readily machined using conventional practices as well as the electrical discharge method (EDM)

Applications:

  • Mold Cores
  • Cavities
  • Sprue Bushings
  • Hot Runner Systems
  • Core Pins
  • Ejector Pins
  • Sleeves
  • Blow Pins

Information provided by Performance Alloys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.315 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 2103000kg
Hardness, Rockwell B 94
Tensile Strength at Break 100000 psi
Tensile Strength, Yield 75.0 ksi
Elongation at Break 13 %in 2"
Compressive Strength 80.0 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.70 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 1800 BTU-in/hr-ft²-°F
@Temperature 15.6 °C
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 0.40 %
Copper, Cu 96.4 %
Nickel, Ni 2.5 %
Silicon, Si 0.70 %
 
Descriptive Properties
Thermal diffusivity at 68°F2.32 ft²/hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
420 Stainless Steel
Performance Alloys MoldStar® 90 Copper Mold Alloy
CoorsTek ACI-Ni10 Tungsten Carbide
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type)
Tungsten Carbide, WC

NPER00 / 18767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.