MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type)
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: PX5 is a modified P20, high performance, high precision, mold steel.

Unique Characteristics:

  • Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots.
  • 30-33 HRc hardness.
  • Uniform hardness throughout, even in heavy sections.
  • 75% tougher than typical chrome-moly steels.
  • Patented chemistry suppresses weld cracking and hardness elevation in the heat affected zone, eliminating the need for pre-heating and post-heating in most welding situations.
  • Machines 30-50% faster than any other P20-type steel.
  • Never needs stress relieving, even after heavy machining.

Applications:
  • plastic molds
  • rubber molds
  • press platens
  • dies

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³literature value
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 30 - 3330 - 33
Tensile Strength, Ultimate 961 MPa139000 psiat Center, Transverse
 961 MPa139000 psiat Center, Longitudinal
 981 MPa142000 psiat Surface, Longitudinal
 981 MPa142000 psiat Surface, Transverse
Tensile Strength, Yield 843 MPa122000 psiat Center, Longitudinal
 843 MPa122000 psiat Center, Transverse
 863 MPa125000 psiat Surface, Transverse
 863 MPa125000 psiat Surface, Longitudinal
Impact 4.64.6(kgf m/cm2), Impact Toughness at Center, Transverse
 4.84.8(kgf m/cm2), Impact Toughness at Surface, Transverse
 6.76.7(kgf m/cm2), Impact Toughness at Center, Longitudinal
 8.28.2(kgf m/cm2), Impact Toughness at Surface, Longitudinal
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.9 µm/m-°C
@Temperature 30.0 - 100 °C
6.60 µin/in-°F
@Temperature 86.0 - 212 °F
 12.8 µm/m-°C
@Temperature 30.0 - 200 °C
7.10 µin/in-°F
@Temperature 86.0 - 392 °F
 13.1 µm/m-°C
@Temperature 30.0 - 300 °C
7.30 µin/in-°F
@Temperature 86.0 - 572 °F
 13.5 µm/m-°C
@Temperature 30.0 - 400 °C
7.50 µin/in-°F
@Temperature 86.0 - 752 °F
 14.0 µm/m-°C
@Temperature 30.0 - 600.0 °C
7.80 µin/in-°F
@Temperature 86.0 - 1112 °F
Specific Heat Capacity  0.473 J/g-°C
@Temperature 20.0 °C
0.113 BTU/lb-°F
@Temperature 68.0 °F
 0.490 J/g-°C
@Temperature 100 °C
0.117 BTU/lb-°F
@Temperature 212 °F
 0.544 J/g-°C
@Temperature 200 °C
0.130 BTU/lb-°F
@Temperature 392 °F
 0.561 J/g-°C
@Temperature 300 °C
0.134 BTU/lb-°F
@Temperature 572 °F
 0.628 J/g-°C
@Temperature 400 °C
0.150 BTU/lb-°F
@Temperature 752 °F
Thermal Conductivity  38.76 W/m-K
@Temperature 400 °C
269.0 BTU-in/hr-ft²-°F
@Temperature 752 °F
 39.20 W/m-K
@Temperature 300 °C
272.0 BTU-in/hr-ft²-°F
@Temperature 572 °F
 42.03 W/m-K
@Temperature 200 °C
291.7 BTU-in/hr-ft²-°F
@Temperature 392 °F
 42.34 W/m-K
@Temperature 100 °C
293.8 BTU-in/hr-ft²-°F
@Temperature 212 °F
 42.42 W/m-K
@Temperature 20.0 °C
294.4 BTU-in/hr-ft²-°F
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
AISI Type P20 Mold Steel (UNS T51620)
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
420 Stainless Steel
Bohler-Uddeholm UDDEHOLM RAMAX® S Modified 420F

NIMS03 / 17382

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.