MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type)
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: PX5 is a modified P20, high performance, high precision, mold steel.

Unique Characteristics:

  • Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots.
  • 30-33 HRc hardness.
  • Uniform hardness throughout, even in heavy sections.
  • 75% tougher than typical chrome-moly steels.
  • Patented chemistry suppresses weld cracking and hardness elevation in the heat affected zone, eliminating the need for pre-heating and post-heating in most welding situations.
  • Machines 30-50% faster than any other P20-type steel.
  • Never needs stress relieving, even after heavy machining.

Applications:
  • plastic molds
  • rubber molds
  • press platens
  • dies

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccliterature value
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 30 - 33
Tensile Strength, Ultimate 9800 kg(f)/cm²at Center, Transverse
 9800 kg(f)/cm²at Center, Longitudinal
 10000 kg(f)/cm²at Surface, Longitudinal
 10000 kg(f)/cm²at Surface, Transverse
Tensile Strength, Yield 8600 kg(f)/cm²at Center, Longitudinal
 8600 kg(f)/cm²at Center, Transverse
 8800 kg(f)/cm²at Surface, Transverse
 8800 kg(f)/cm²at Surface, Longitudinal
Impact 4.6(kgf m/cm2), Impact Toughness at Center, Transverse
 4.8(kgf m/cm2), Impact Toughness at Surface, Transverse
 6.7(kgf m/cm2), Impact Toughness at Center, Longitudinal
 8.2(kgf m/cm2), Impact Toughness at Surface, Longitudinal
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.60 µin/in-°F
@Temperature 30.0 - 100 °C
 7.10 µin/in-°F
@Temperature 30.0 - 200 °C
 7.30 µin/in-°F
@Temperature 30.0 - 300 °C
 7.50 µin/in-°F
@Temperature 30.0 - 400 °C
 7.80 µin/in-°F
@Temperature 30.0 - 600.0 °C
Specific Heat Capacity 0.113 BTU/lb-°F
@Temperature 20.0 °C
 0.117 BTU/lb-°F
@Temperature 100 °C
 0.130 BTU/lb-°F
@Temperature 200 °C
 0.134 BTU/lb-°F
@Temperature 300 °C
 0.150 BTU/lb-°F
@Temperature 400 °C
Thermal Conductivity 269.0 BTU-in/hr-ft²-°F
@Temperature 400 °C
 272.0 BTU-in/hr-ft²-°F
@Temperature 300 °C
 291.7 BTU-in/hr-ft²-°F
@Temperature 200 °C
 293.8 BTU-in/hr-ft²-°F
@Temperature 100 °C
 294.4 BTU-in/hr-ft²-°F
@Temperature 20.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
AISI Type P20 Mold Steel (UNS T51620)
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
420 Stainless Steel
Bohler-Uddeholm UDDEHOLM RAMAX® S Modified 420F

NIMS03 / 17382

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.