MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Röchling Polystone® PPs EL black Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product characteristics:
  • Antistatic
  • Flame retardant
  • Electrically conductive
Product applications:
  • Ventilation technology
  • Pump engineering
  • Electrical industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³DIN EN ISO 1183-1
Water Absorption <= 0.10 %<= 0.10 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767DIN EN ISO 868
Tensile Strength, Yield 20.0 MPa2900 psiDIN EN ISO 527
Elongation at Break >= 20 %>= 20 %DIN EN ISO 527
Modulus of Elasticity 1.40 GPa203 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) >= 4.00 kJ/m²>= 1.90 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10000 ohm-cm<= 10000 ohm-cmDIN EN 62631-3-1
Surface Resistance <= 10000 ohm<= 10000 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 - 190 µm/m-°C66.7 - 106 µin/in-°FDIN 53752
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°FDIN 52612
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 145 °C293 °FISO 11357-3
Maximum Service Temperature, Air 80.0 °C176 °Flong term
 130 °C266 °Fshort term
Vicat Softening Point 81.0 °C178 °FDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air 0.000 °C32.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PPS-GF40-01 AD3002 Black PPS, 40% Glass Reinforced
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black
Aurora Plastics TufFill™ 5000-SN4 PP, Flame Retardant

PROCH9266 / 232969

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.