MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celstran® PPS-GF40-01 AD3002 Black PPS, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: 40% long strand fiber glass reinforced polyphenylene sulfide

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.62 g/cc1.62 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 155 MPa22500 psi5mm/min; ISO 527-2/1A
 176 MPa25500 psiASTM D638
 59.3 MPa
@Temperature 204 °C
8600 psi
@Temperature 400 °F
ASTM D638
 84.1 MPa
@Temperature 149 °C
12200 psi
@Temperature 300 °F
ASTM D638
 179 MPa
@Temperature -40.0 °C
26000 psi
@Temperature -40.0 °F
ASTM D638
Elongation at Break 1.11 %1.11 %5mm/min; ISO 527-2/1A
 1.2 %1.2 %ASTM D638
 1.16 %
@Temperature 4.44 °C
1.16 %
@Temperature 40.0 °F
ASTM D638
 1.25 %
@Temperature 204 °C
1.25 %
@Temperature 400 °F
ASTM D638
 1.35 %
@Temperature 149 °C
1.35 %
@Temperature 300 °F
ASTM D638
Tensile Modulus 15.858 GPa2300.0 ksi50mm/min; ISO 527-2/1A
 16.8 GPa2430 ksiASTM D638
 7.93 GPa
@Temperature 204 °C
1150 ksi
@Temperature 400 °F
ASTM D638
 8.62 GPa
@Temperature 149 °C
1250 ksi
@Temperature 300 °F
ASTM D638
 17.8 GPa
@Temperature -40.0 °C
2580 ksi
@Temperature -40.0 °F
ASTM D638
Flexural Strength 248 MPa36000 psiISO 178
 248 MPa36000 psiASTM D790
 127 MPa
@Temperature 204 °C
18400 psi
@Temperature 400 °F
ASTM D790
 159 MPa
@Temperature 149 °C
23000 psi
@Temperature 300 °F
ASTM D790
 256 MPa
@Temperature -40.0 °C
37200 psi
@Temperature -40.0 °F
ASTM D790
Flexural Modulus 14.1 GPa2040 ksiASTM D790
 14.86 GPa2155 ksiISO 178
 6.21 GPa
@Temperature 204 °C
900 ksi
@Temperature 400 °F
ASTM D790
 7.58 GPa
@Temperature 149 °C
1100 ksi
@Temperature 300 °F
ASTM D790
 15.0 GPa
@Temperature -40.0 °C
2170 ksi
@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 3.42 J/cm6.40 ft-lb/inASTM D256
 3.42 J/cm
@Temperature -40.0 °C
6.40 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Charpy Impact, Notched 2.20 J/cm²10.5 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 279 °C535 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 160 °C284 - 320 °Fcavity
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 285 - 295 °C545 - 563 °F
Zone 2 290 - 300 °C554 - 572 °F
Zone 3 295 - 305 °C563 - 581 °F
Zone 4 300 - 310 °C572 - 590 °F
Die Temperature 290 - 300 °C554 - 572 °F
Melt Temperature 300 - 310 °C572 - 590 °F
Drying Temperature 130 - 140 °C266 - 284 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PPS-GF40-01 PPS, 40% Glass Reinforced
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose
Techmer ES HiFill® PPS GF40 BK 40% Glass Filled
Omnia Plastica PPS GF40 Polyphenylenesulphide
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

PHCQ250 / 178705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.