MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epoxy and polyurethane coatings. It is an excellent tie-coat between old glossy epoxy and other cured coating for subsequent coatings. It offers the best recoat adhesion within the first 1-4 days. After this point, it should be sanded or reprimed with Primkote G if it is glossy and difficult to wet. It can also be used alone, in one or several coats, to protect a color pattern, etc. Primkote G offers: (1) Application to freshly poured concrete, within hours after the concrete has been poured; (2) Application to fully cured concrete; (3) Cancels out the necessity to wait 28 days or cure and shot-blast new concrete before it can be finished; (4) Very low viscosity for penetration and wetting; (5) Low VOC (meets EPA method 24); (6) Outstanding water and weather resistance; (7) Fast hardening time (1 1/4 hrs); (8) Gray color for improved visual inspection. Suggested Uses: Priming/Sealing of freshly poured concrete surfaces; Penetrating and Conditioning concrete for urethanes and tie-coats on epoxy surfaces; Gray-Colored Primer for floors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
Density 8.11 lb/gal
Solids Content 41.2 %
Viscosity 10.5 - 18 cP
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 45.0 min
Pot Life 720 min
 
Descriptive Properties
Hardening Time (min)7525°C
Hardness, pencilHB
Parts by Weight (pbw)100Part A
 54.4Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Concrete, foamed blast furnace slag aggregate
Autoclaved aerated concrete, 0.800 g/cc density
Concrete, Lightweight
ChevronTexaco Concrete Form Oil VOC
Mitsubishi Chemical Advanced Materials Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite

PABC837 / 107821

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.