MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DUREFLEX® PS5400 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characterization: The Dureflex PS5400 Series is a family of aromatic polyester polyurethane film/sheet products.

Properties/Applications: Desmotherm® 2170 is used primarily as the binder in one-component stoving polyurethane systems for highly flexible primers, intermediate coats, primer surfacers and thin coil-coating primers. Being a self-crosslinking stoving urethane resin, the product contains the amount of polyol required for crosslinking as well as the hardener. The film properties can be modified by combination with various polyesters from the Desmophen® and Alkynol® ranges, amino resins and flexibilisers. The main field of application for systems based on Desmotherm® 2170 is as primer surfacers in automotive OEM finishing. When formulating coatings with Desmotherm® 2170, the temperature should not exceed 60 °C otherwise the crosslinking reaction will begin.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength, Ultimate 8300 psiMD/CD Ave; ASTM D882
Elongation at Yield 650 %Ultimate; ASTM D882
100% Modulus 0.00621 GPa
@Strain 100 %
MD/CD Ave; ASTM D882
300% Modulus 0.0117 GPa
@Strain 300 %
MD/CD Ave; ASTM D882
Tear Strength 600 pliMD/CD Ave; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
Softening Point 108 - 132 °CASTM E2347-004

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DUREFLEX® PT6400 TPU
Covestro DUREFLEX® PS7000 TPU
Covestro DUREFLEX® PS8400 TPU
Covestro DUREFLEX® X2103 TPU
Covestro DUREFLEX® PS8000 TPU

PCOVEST0760 / 202543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.