MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Trelleborg R940 Natural Rubber Polyisoprene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

All information provided by Trelleborg

Key Words: NR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090
Tensile Strength, Yield 13.5 MPa1960 psi
Elongation at Break 220 %220 %
Tear Strength 29.0 kN/m165 pli
Abrasion 120120mm3; 10 N Load
Compression Set 50 %
@Temperature 70.0 °C,
Time 79200 sec
50 %
@Temperature 158 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)

PTRELL028 / 83786

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.