MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Skybond® 703 Aromatic Polyimide Resin for Composites
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: SKYBOND® 703 is a heat reactive aromatic resin which can be thermally cured to a crosslinked polyimide. It is specifically designed for structural and specialty applications where extended exposure to temperatures up to 650°F is required.

Information provided by Industrial Summit Technology Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.18 g/cc0.0415 - 0.0426 lb/in³
Solids Content 48 - 51 %48 - 51 %
Viscosity 3000 - 7000 cP3000 - 7000 cP
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 343 °C650 °FLaminate strength retained

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Skybond® 705 Aromatic Polyimide Resin for Coatings
Skybond® 701 Aromatic Polyimide Resin
Solvay CYCOM® 2237 Polyimide Resin System
Overview of materials for Polyimide
NeXolve Novastrat® 905 Polyimide

PISTEC952 / 183040

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.