MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.00 - 1.60 g/ccAverage value: 1.14 g/cc Grade Count:539
Filler Content 25.0 - 33.0 %Average value: 29.6 % Grade Count:136
Water Absorption 0.000 - 2.00 %Average value: 0.0499 % Grade Count:71
Moisture Absorption at Equilibrium 0.0100 - 0.100 %Average value: 0.0460 % Grade Count:5
Water Absorption at Saturation 0.100 - 0.200 %Average value: 0.138 % Grade Count:4
Additive Loading 30.0 %Average value: 30.0 % Grade Count:10
Maximum Moisture Content 0.0100 - 0.200Average value: 0.105 Grade Count:6
 0.200 - 0.200
@Temperature 120 - 120 °C
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000600 - 0.0350 cm/cmAverage value: 0.00401 cm/cm Grade Count:324
 0.00400 - 0.00400 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00356 cm/cm Grade Count:1
 0.00350 - 0.00350 cm/cm
@Temperature 220 - 240 °C
Average value: 0.00356 cm/cm Grade Count:4
 0.00350 - 0.00350 cm/cm
@Pressure 60.0 - 60.0 MPa
Average value: 0.00356 cm/cm Grade Count:4
Linear Mold Shrinkage, Transverse 0.000800 - 0.0193 cm/cmAverage value: 0.00782 cm/cm Grade Count:99
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00800 cm/cm Grade Count:1
Melt Flow 0.300 - 25.0 g/10 minAverage value: 7.66 g/10 min Grade Count:404
Spiral Flow 95.0 - 95.0 cm
@Temperature 250 - 250 °C
Average value: 95.0 cm Grade Count:1
 95.0 - 95.0 cm
@Thickness 2.00 - 2.00 mm
Average value: 95.0 cm Grade Count:1
Ash 26.0 - 34.0 %Average value: 30.0 % Grade Count:26
 28.0 - 32.0 %
@Temperature 600 - 700 °C
Average value: 30.0 % Grade Count:6
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 57.0 - 107Average value: 66.7 Grade Count:9
Hardness, Rockwell R 81.0 - 115Average value: 100 Grade Count:64
Hardness, Shore D 47.0 - 85.0Average value: 72.8 Grade Count:29
Ball Indentation Hardness 64.0 - 132 MPaAverage value: 111 MPa Grade Count:8
Tensile Strength, Ultimate 6.89 - 180 MPaAverage value: 81.3 MPa Grade Count:314
 9.00 - 140.653 MPa
@Temperature -40.0 - 120 °C
Average value: 58.0 MPa Grade Count:30
Tensile Strength, Yield 6.20 - 111 MPaAverage value: 75.2 MPa Grade Count:223
Elongation at Break 0.900 - 98.0 %Average value: 4.73 % Grade Count:335
 1.30 - 7.50 %
@Temperature -40.0 - 100 °C
Average value: 3.08 % Grade Count:27
Elongation at Yield 2.00 - 9.40 %Average value: 3.56 % Grade Count:78
 2.50 - 4.00 %
@Temperature 60.0 - 90.0 °C
Average value: 3.25 % Grade Count:1
Modulus of Elasticity 2.25 - 15.0 GPaAverage value: 6.33 GPa Grade Count:225
 3.30 - 11.0 GPa
@Temperature -40.0 - 100 °C
Average value: 5.19 GPa Grade Count:27
Flexural Yield Strength 32.0 - 260 MPaAverage value: 118 MPa Grade Count:322
 70.0 - 234.422 MPa
@Temperature -40.0 - 121 °C
Average value: 112 MPa Grade Count:23
Flexural Modulus 0.115 - 8.85 GPaAverage value: 5.25 GPa Grade Count:504
 1.60 - 8.34266 GPa
@Temperature -40.0 - 121 °C
Average value: 4.91 GPa Grade Count:26
Compressive Yield Strength 57.9 - 82.7 MPaAverage value: 71.7 MPa Grade Count:7
Izod Impact, Notched 0.320 - 4.15 J/cmAverage value: 1.12 J/cm Grade Count:254
 0.300 - 4.35 J/cm
@Temperature -40.0 - 121 °C
Average value: 1.39 J/cm Grade Count:27
 0.5339 - 0.5339 J/cm
@Temperature -28.9 - -28.9 °C
Average value: 1.39 J/cm Grade Count:1
 0.5339 - 0.5339 J/cm
@Thickness 3.17 - 3.17 mm
Average value: 1.39 J/cm Grade Count:1
Izod Impact, Unnotched 0.650 - 8.54 J/cmAverage value: 5.12 J/cm Grade Count:81
 0.450 - 1.10 J/cm
@Temperature 0.000 - 0.000 °C
Average value: 0.788 J/cm Grade Count:4
Izod Impact, Notched (ISO) 4.50 - 55.0 kJ/m²Average value: 13.3 kJ/m² Grade Count:93
 4.41 - 50.0 kJ/m²
@Temperature -45.0 - -20.0 °C
Average value: 11.0 kJ/m² Grade Count:21
Izod Impact, Unnotched (ISO) 18.0 - 21000 kJ/m²Average value: 41.9 kJ/m² Grade Count:13
 18.0 - 68.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 41.4 kJ/m² Grade Count:5
Charpy Impact Unnotched 0.500 - 2100 J/cm²Average value: 4.85 J/cm² Grade Count:156
 0.400 - 8.70 J/cm²
@Temperature -45.0 - 0.000 °C
Average value: 4.40 J/cm² Grade Count:80
Charpy Impact, Notched 0.280 - 5.00 J/cm²Average value: 1.61 J/cm² Grade Count:225
 0.100 - 3.50 J/cm²
@Temperature -40.0 - 0.000 °C
Average value: 1.23 J/cm² Grade Count:126
Gardner Impact 0.300 - 23.0 JAverage value: 2.05 J Grade Count:38
 2.71164 - 2.71164 J
@Temperature -5.56 - -5.56 °C
Average value: 2.71 J Grade Count:1
Puncture Energy 21.0 - 21.0 J
@Temperature -30.0 - -30.0 °C
Average value: 21.0 J Grade Count:1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1000 - 3.00e+16 ohm-cmAverage value: 3.44e+15 ohm-cm Grade Count:35
Surface Resistance 1e+05 - 1.60e+15 ohmAverage value: 5.98e+14 ohm Grade Count:20
Dielectric Constant 2.50 - 3.30Average value: 2.77 Grade Count:20
Dielectric Strength 17.7 - 40.0 kV/mmAverage value: 25.0 kV/mm Grade Count:22
Dissipation Factor 0.00100 - 0.00300Average value: 0.00158 Grade Count:12
Arc Resistance 85.0 - 125 secAverage value: 109 sec Grade Count:8
Comparative Tracking Index 575 - 650 VAverage value: 612 V Grade Count:32
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.00 - 72.0 µm/m-°CAverage value: 42.3 µm/m-°C Grade Count:38
Thermal Conductivity 0.270 - 0.331 W/m-KAverage value: 0.319 W/m-K Grade Count:9
Melting Point 145 - 220 °CAverage value: 164 °C Grade Count:76
Maximum Service Temperature, Air 65.0 - 160 °CAverage value: 117 °C Grade Count:12
Hot Ball Pressure Test 125 - 145 °CAverage value: 129 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 99.0 - 165 °CAverage value: 153 °C Grade Count:242
Deflection Temperature at 1.8 MPa (264 psi) 63.9 - 220 °CAverage value: 143 °C Grade Count:407
Deflection Temperature at 8.0 MPa 117 - 134 °CAverage value: 122 °C Grade Count:21
Vicat Softening Point 85.0 - 166 °CAverage value: 137 °C Grade Count:192
UL RTI, Electrical 65.0 - 230 °CAverage value: 88.6 °C Grade Count:7
UL RTI, Mechanical with Impact 65.0 - 230 °CAverage value: 88.6 °C Grade Count:7
UL RTI, Mechanical without Impact 65.0 - 230 °CAverage value: 88.6 °C Grade Count:7
Flammability, UL94 HB - 5VAGrade Count:214
Flame Spread 9.00 - 100 mm/minAverage value: 29.0 mm/min Grade Count:11
Oxygen Index 20.0 - 29.0 %Average value: 22.1 % Grade Count:18
Glow Wire Test 550 - 960 °CAverage value: 765 °C Grade Count:50
 
Processing PropertiesOriginal ValueComments
Processing Temperature 30.0 - 270 °CAverage value: 170 °C Grade Count:68
Nozzle Temperature 188 - 270 °CAverage value: 231 °C Grade Count:64
Die Temperature 200 - 270 °CAverage value: 241 °C Grade Count:34
Melt Temperature 145 - 302 °CAverage value: 229 °C Grade Count:253
Mold Temperature 4.00 - 100 °CAverage value: 52.7 °C Grade Count:259
Injection Velocity 13.0 - 200 mm/secAverage value: 98.4 mm/sec Grade Count:11
Drying Temperature 48.9 - 220 °CAverage value: 86.1 °C Grade Count:205
Moisture Content 0.0200 - 0.200 %Average value: 0.128 % Grade Count:68
Injection Pressure 2.76 - 130 MPaAverage value: 75.4 MPa Grade Count:127
Hot-Working Temperature 230 - 270 °CAverage value: 253 °C Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Overview of materials for Polypropylene with 40% Glass Fiber Filler
Overview of materials for Polypropylene with 60% Glass Fiber Filler

O4713 / 78378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.