MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 60 H2.0 EF DUS060 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: PA 6, 60% glass fibers, injection molding, improved flowability, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccISO 1183
Moisture Absorption at Equilibrium 1.3 %50% RH; ISO 62
Water Absorption at Saturation 3.6 %IOS 62
Linear Mold Shrinkage, Flow 0.0032 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 155 MPaISO 2093-1
Tensile Strength at Break 145 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 3.5 %5 mm/min; ISO 527-1,-2
Tensile Modulus 12000 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 235 MPa2 mm/min; ISO 178-A
Flexural Modulus 12800 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 3.6 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 20.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 80.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
 90.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+9 ohm-cmIEC 60093
Dielectric Constant 5.1
@Frequency 1e+6 Hz
IEC 60250
 11.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0651
@Frequency 1e+6 Hz
IEC 60250
 0.2149
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °Cinjection molding
 270 - 290 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 60 H2.0 EF DUS060 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Dry
Domo TechnylStar™ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY
Domo TechnylStar™ SX 218 V50 PA6, 50% glass filled
Domo TechnylStar™ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY
Envalior Durethan® BKV 30 G H2.0 900051 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry

PLANW9435 / 208266

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.