Physical Properties | Metric | English | Comments |
---|
Density | 7.80 g/cc | 0.282 lb/in³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Brinell | 140 - 190 @Thickness <=16.0 mm | 140 - 190 @Thickness <=0.630 in |
| 140 - 190 @Thickness 16.0 - 40.0 mm | 140 - 190 @Thickness 0.630 - 1.57 in |
| 140 - 190 @Thickness 40.0 - 63.0 mm | 140 - 190 @Thickness 1.57 - 2.48 in |
| 140 - 190 @Thickness 63.0 - 80.0 mm | 140 - 190 @Thickness 2.48 - 3.15 in |
| 140 - 190 @Thickness 80.0 - 100 mm | 140 - 190 @Thickness 3.15 - 3.94 in |
Tensile Strength | 470 - 630 MPa @Thickness <=16.0 mm | 68200 - 91400 psi @Thickness <=0.630 in |
| 470 - 630 MPa @Thickness 16.0 - 40.0 mm | 68200 - 91400 psi @Thickness 0.630 - 1.57 in |
| 470 - 630 MPa @Thickness 40.0 - 63.0 mm | 68200 - 91400 psi @Thickness 1.57 - 2.48 in |
| 470 - 630 MPa @Thickness 63.0 - 80.0 mm | 68200 - 91400 psi @Thickness 2.48 - 3.15 in |
| 470 - 630 MPa @Thickness 80.0 - 100 mm | 68200 - 91400 psi @Thickness 3.15 - 3.94 in |
Tensile Strength, Yield | >= 315 MPa @Thickness 80.0 - 100 mm | >= 45700 psi @Thickness 3.15 - 3.94 in |
| >= 325 MPa @Thickness 63.0 - 80.0 mm | >= 47100 psi @Thickness 2.48 - 3.15 in |
| >= 335 MPa @Thickness 40.0 - 63.0 mm | >= 48600 psi @Thickness 1.57 - 2.48 in |
| >= 345 MPa @Thickness 16.0 - 40.0 mm | >= 50000 psi @Thickness 0.630 - 1.57 in |
| >= 355 MPa @Thickness <=16.0 mm | >= 51500 psi @Thickness <=0.630 in |
Elongation at Break | 20 % @Thickness 63.0 - 80.0 mm | 20 % @Thickness 2.48 - 3.15 in |
| 20 % @Thickness 80.0 - 100 mm | 20 % @Thickness 3.15 - 3.94 in |
| 21 % @Thickness 40.0 - 63.0 mm | 21 % @Thickness 1.57 - 2.48 in |
| 22 % @Thickness <=16.0 mm | 22 % @Thickness <=0.630 in |
| 22 % @Thickness 16.0 - 40.0 mm | 22 % @Thickness 0.630 - 1.57 in |
Modulus of Elasticity | 210 GPa | 30500 ksi |
Poissons Ratio | 0.30 | 0.30 |
Shear Modulus | 80.0 GPa | 11600 ksi |
Impact Test | 27.0 J @Thickness <=16.0 mm, Temperature -20.0 °C | 19.9 ft-lb @Thickness <=0.630 in, Temperature -4.00 °F |
| 27.0 J @Thickness 16.0 - 40.0 mm, Temperature -20.0 °C | 19.9 ft-lb @Thickness 0.630 - 1.57 in, Temperature -4.00 °F |
| 27.0 J @Thickness 40.0 - 63.0 mm, Temperature -20.0 °C | 19.9 ft-lb @Thickness 1.57 - 2.48 in, Temperature -4.00 °F |
| 27.0 J @Thickness 63.0 - 80.0 mm, Temperature -20.0 °C | 19.9 ft-lb @Thickness 2.48 - 3.15 in, Temperature -4.00 °F |
| 27.0 J @Thickness 80.0 - 100 mm, Temperature -20.0 °C | 19.9 ft-lb @Thickness 3.15 - 3.94 in, Temperature -4.00 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 0.00000200 - 0.00000250 ohm-cm | 0.00000200 - 0.00000250 ohm-cm |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 300 °C | 6.67 µin/in-°F @Temperature 68.0 - 572 °F |
Specific Heat Capacity | 0.460 - 0.480 J/g-°C @Temperature 50.0 - 100 °C | 0.110 - 0.115 BTU/lb-°F @Temperature 122 - 212 °F |
Thermal Conductivity | 40.0 - 45.0 W/m-K | 278 - 312 BTU-in/hr-ft²-°F |
Transformation Temperature | 400 °C | 752 °F |
| 720 °C | 1330 °F |
| 815 °C | 1500 °F |
|
Component Elements Properties | Metric | English | Comments |
---|
Carbon, C | <= 0.24 % | <= 0.24 % |
Copper, Cu | <= 0.55 % | <= 0.55 % |
Iron, Fe | >= 97.01 % | >= 97.01 % |
Manganese, Mn | <= 1.6 % | <= 1.6 % |
Phosphorus, P | <= 0.025 % | <= 0.025 % |
Silicon, Si | <= 0.55 % | <= 0.55 % |
Sulfur, S | <= 0.025 % | <= 0.025 % |
|
Descriptive Properties |
---|
Weldability | CEV 0.52max |
| Pcm 0.35max |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view