MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 333.0-T5, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 333.0-T5; UNS A03330; AA333.0-T5. Comparable to JIS AC4B. AlSi8Cu3; Al333.0-T5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.77 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 70 - 105AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 112Estimated from Brinell Hardness.
Hardness, Rockwell A 37Estimated from Brinell Hardness.
Hardness, Rockwell B 55Estimated from Brinell Hardness.
Hardness, Vickers 99Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 30.0 ksiAA
Tensile Modulus 73.0 GPaEstimated from 360.0
Poissons Ratio 0.33Estimated from 360.0
Machinability 50 %0-100 Scale (100=best)
Shear Modulus 27.4 GPaCalculated
Shear Strength 127 MPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000590 ohm-cmAA; Typical 29% IACS Conductivity
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 11.4 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical
 12.4 µin/in-°F
@Temperature 20.0 - 300 °C
AA; Typical; average over range
Specific Heat Capacity 0.963 J/g-°CTypical for cast aluminum
Thermal Conductivity 0.280 cal cm/sec-cm²-°CAA; Typical at 25°C
Melting Point 960 - 1085 °FAA; Typical
Solidus 960 °FAA; Typical
Liquidus 1085 °FAA; Typical
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 81.8 - 89 %As remainder
Copper, Cu 3.0 - 4.0 %
Iron, Fe <= 1.0 %
Magnesium, Mg 0.05 - 0.50 %
Manganese, Mn <= 0.50 %
Nickel, Ni <= 0.50 %
Other, total <= 0.50 %
Silicon, Si 8.0 - 10 %
Titanium, Ti <= 0.25 %
Zinc, Zn <= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 333.0-F, Permanent Mold Cast
Aluminum A413.0-F Die Casting Alloy
Aluminum 333.0-T6, Permanent Mold Cast
Aluminum 333.0-T7, Permanent Mold Cast
Aluminum 413.0-F Die Casting Alloy

MAC3330T5 / 9880

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.