MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aluminum Castings

Aluminum 413.0-F Die Casting Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 413.0-F; UNS A04130; AA413.0-F Die, ISO 3522 AlSi12CuFe and AlSi12Fe. ISO R164 AlSi12, AlSi12Cu, AlSi12CuFe, AlSi12Fe. ISO R2147 AlSi12, EN 1706 AC 44100, BB401, CC401, EA401, G-AlSi12, DIN 230, UNI 4514, AS 13, RSA SA 22, 12Si. Comparable to; Al413.0-F
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0961 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8080
Tensile Strength, Ultimate 296 MPa42900 psi
Tensile Strength, Yield 145 MPa
@Strain 0.2 %
21000 psi
@Strain 0.2 %
Elongation at Break 2.5 %2.5 %in 50 mm
Modulus of Elasticity 71.0 GPa10300 ksi
Poissons Ratio 0.330.33
Fatigue Strength 130 MPa
@# of Cycles 5.00e+8
18900 psi
@# of Cycles 5.00e+8
Notch Status unknown, R.R. Moore Test
Machinability 30 %30 %0-100 Scale (100=best)
Shear Modulus 26.7 GPa3870 ksiCalculated
Shear Strength 170 MPa24700 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000440 ohm-cm0.00000440 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lb
CTE, linear  20.4 µm/m-°C
@Temperature 20.0 - 100 °C
11.3 µin/in-°F
@Temperature 68.0 - 212 °F
 22.4 µm/m-°C
@Temperature 20.0 - 300 °C
12.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°F
Thermal Conductivity 121 W/m-K840 BTU-in/hr-ft²-°F
Melting Point 574 - 582 °C1070 - 1080 °F
Solidus 574 °C1070 °F
Liquidus 582 °C1080 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 649 - 760 °C1200 - 1400 °F
Casting Temperature 635.0 - 704 °C1175 - 1300 °FDie Casting
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 82.2 - 89 %82.2 - 89 %As remainder
Copper, Cu <= 1.0 %<= 1.0 %
Iron, Fe <= 2.0 %<= 2.0 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Manganese, Mn <= 0.35 %<= 0.35 %
Nickel, Ni <= 0.50 %<= 0.50 %
Other, total <= 0.25 %<= 0.25 %
Silicon, Si 11 - 13 %11 - 13 %
Tin, Sn <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.50 %<= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A413.0-F Die Casting Alloy
Aluminum A380.1 Composition Spec
Aluminum 384.0-F Die Casting Alloy
Overview of materials for Hot Work Steel
Aluminum A380.0-F Die Casting Alloy

MAC4130F / 10088

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.