MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics WDS® Flexible Design Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: WDS® Flexible Design is a microporous insulation material with an extremely low coefficient of thermal conductivity, i.e. with very good insulating properties. WDS® Flexible Design consists of inorganic oxides. The main constituent is fumed silica, the other components are opacifiers for minimizing infrared radiation, and reinforcing glass filaments. WDS® Flexible Design (core material) is not flammable and meets the requirements of IMO FTPC part 1 and DIN EN 13501-1, class A1. WDS® Flexible Design is heat sealed in a close-fitting 15µm PE shrink film.

Application: WDS® Flexible Design was specially developed for applications in the automotive industry. In this case, specifically for automotive exhaust systems. The significant reduction of the required insulation thicknesses with WDS® Flexible Design leads to highly efficient weight and space saving thermal insulation.

Information provided by Morgan Advanced Materials

Key Words: Porextherm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.185 - 0.250 g/ccnominal
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.470 BTU/lb-°F
@Temperature 700.0 °C
Thermal Conductivity 0.0210 W/m-K
@Temperature 20.0 °C
ASTM C177
 0.0240 W/m-K
@Temperature 200 °C
ASTM C177
 0.0270 W/m-K
@Temperature 400 °C
ASTM C177
 0.0350 W/m-K
@Temperature 600 °C
ASTM C177
 0.0450 W/m-K
@Temperature 800 °C
ASTM C177
Shrinkage 1.5 %
@Treatment Temp. 950 °C,
Time 86400 sec
full soak
 3.9 %
@Treatment Temp. 1000 °C,
Time 86400 sec
full soak
 
Component Elements PropertiesOriginal ValueComments
Other 5.0 %
SiC 15 %
SiO2 80 %
 
Descriptive Properties
Classification Temperature (°C)1000
Colorgrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper
Thermal Ceramics BTU-GUE
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
3M 4317 Single-Coated Foam Tape

CMORF6119 / 202903

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.