MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Morgan Advanced Ceramics WDS® Flexible Design Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: WDS® Flexible Design is a microporous insulation material with an extremely low coefficient of thermal conductivity, i.e. with very good insulating properties. WDS® Flexible Design consists of inorganic oxides. The main constituent is fumed silica, the other components are opacifiers for minimizing infrared radiation, and reinforcing glass filaments. WDS® Flexible Design (core material) is not flammable and meets the requirements of IMO FTPC part 1 and DIN EN 13501-1, class A1. WDS® Flexible Design is heat sealed in a close-fitting 15µm PE shrink film.

Application: WDS® Flexible Design was specially developed for applications in the automotive industry. In this case, specifically for automotive exhaust systems. The significant reduction of the required insulation thicknesses with WDS® Flexible Design leads to highly efficient weight and space saving thermal insulation.

Information provided by Morgan Advanced Materials

Key Words: Porextherm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.185 - 0.250 g/cc0.00668 - 0.00903 lb/in³nominal
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.97 J/g-°C
@Temperature 700.0 °C
0.470 BTU/lb-°F
@Temperature 1292 °F
Thermal Conductivity  0.0210 W/m-K
@Temperature 20.0 °C
0.146 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
ASTM C177
 0.0240 W/m-K
@Temperature 200 °C
0.167 BTU-in/hr-ft²-°F
@Temperature 392 °F
ASTM C177
 0.0270 W/m-K
@Temperature 400 °C
0.187 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C177
 0.0350 W/m-K
@Temperature 600 °C
0.243 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C177
 0.0450 W/m-K
@Temperature 800 °C
0.312 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C177
Shrinkage  1.5 %
@Treatment Temp. 950 °C,
Time 86400 sec
1.5 %
@Treatment Temp. 1740 °F,
Time 24.0 hour
full soak
 3.9 %
@Treatment Temp. 1000 °C,
Time 86400 sec
3.9 %
@Treatment Temp. 1830 °F,
Time 24.0 hour
full soak
 
Component Elements PropertiesMetricEnglishComments
Other 5.0 %5.0 %
SiC 15 %15 %
SiO2 80 %80 %
 
Descriptive Properties
Classification Temperature (°C)1000
Colorgrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper
Thermal Ceramics BTU-GUE
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
3M 4317 Single-Coated Foam Tape

CMORF6119 / 202903

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.