MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
International Mold Steel TOOLOX® 44 Plastic and Rubber Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: TOOLOX 44 is a new quenched and tempered tool steel designed to have high impact and low residual stresses and therefore good dimensional stability. Applications include: Machine components; Wear components; Plastic molds; Rubber molds; Press forming; Die cast dies; Forging dies; Coreboxes; Permanent molds

Information provided by International Mold Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 41 - 47
Charpy Impact, Unnotched >= 14.0 ft-lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
International Mold Steel TOOLOX® 33 Cold Work Die Steel
CHT Group MM903 Condensation Cure 2-Part Molding Rubber
CHT Group QGel 323Y High Strength, Fast Curing Silicone Gel
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round

NIMSA02 / 175982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.