MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

International Mold Steel TOOLOX® 33 Cold Work Die Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel

Material Notes: TOOLOX 33 is a quenched and tempered tool steel designed to have low residual stresses and extremely good machinability. Applications include: Plastic molds; Rubber molds; Bending tools; Machine components

Testing in accordance with EN 10 137-1, 10 137-2 and EN ISO 6506-1. Hardness measured on a milled surface, 0,5-2 mm below surface.

Information provided by International Mold Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 280 - 330280 - 330
Hardness, Rockwell C 30 - 3530 - 35
Tensile Strength 896 - 979 MPa130000 - 142000 psi
Charpy Impact, Unnotched 100 - 180 J74.0 - 133 ft-lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
International Mold Steel TOOLOX® 44 Plastic and Rubber Mold Steel
AISI Type H13 Hot Work Tool Steel
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
AISI Type P20 Mold Steel (UNS T51620)
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel

NIMSA03 / 175983

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.