MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC VALOX™ FR DR48 PBT (Asia)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX DR48 is a 17% glass filled, flame retardant Polybutyleneterephthalate (PBT) injection moldable grade with excellent chemical resistance. It has a UL94V0@0.90mm and 5VA@3.0mm flame rating. This is a good candidate for a variety of applications in the electrical industry including connectors, bobbins, and switches.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/ccASTM D792
 1.53 g/cc1.53 g/ccASTM D792
Water Absorption 0.070 %0.070 %24 hours; ASTM D570
Linear Mold Shrinkage, Flow  0.0040 - 0.0060 cm/cm
@Thickness 1.50 - 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.0591 - 0.126 in
SABIC method
 0.0060 - 0.0090 cm/cm
@Thickness 3.20 - 4.60 mm
0.0060 - 0.0090 in/in
@Thickness 0.126 - 0.181 in
SABIC method
Linear Mold Shrinkage, Transverse  0.0050 - 0.0080 cm/cm
@Thickness 1.50 - 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.0591 - 0.126 in
SABIC method
 0.0080 - 0.011 cm/cm
@Thickness 3.20 - 4.60 mm
0.0080 - 0.011 in/in
@Thickness 0.126 - 0.181 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 93.0 MPa13500 psi5 mm/min; ASTM D638
Flexural Strength 140 MPa20300 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.20 GPa754 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.490 J/cm0.918 ft-lb/inASTM D256
Izod Impact, Unnotched 5.00 J/cm9.37 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant  3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
ASTM D150
 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
ASTM D150
Dielectric Strength  18.8 kV/mm
@Thickness 3.20 mm
478 kV/in
@Thickness 0.126 in
in air; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
635 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
ASTM D150
 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  19.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 19.8 µm/m-°C
@Temperature 60.0 - 138 °C
11.0 µin/in-°F
@Temperature 140 - 280 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
@Thickness 6.40 mm
410 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 182 °C
@Thickness 6.40 mm
360 °F
@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 120 °C248 °FUL 746B
UL RTI, Mechanical with Impact 120 °C248 °FUL 746B
UL RTI, Mechanical without Impact 140 °C284 °FUL 746B
Flammability, UL94  V-0
@Thickness 0.900 mm
V-0
@Thickness 0.0354 in
UL 94
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL 94
Oxygen Index 29 %29 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 260 °C473 - 500 °FInjection Molding
Zone 1 240 - 255 °C464 - 491 °F
Zone 2 245 - 260 °C473 - 500 °F
Zone 3 250 - 265 °C482 - 509 °F
Melt Temperature 250 - 265 °C482 - 509 °F
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 12.0 hour12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00250 - 0.00380 cm0.000984 - 0.00150 in
Screw Speed 50 - 80 rpm50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10346 / 243813

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.