MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G HS BK-106. In parts containing cross sections, significant pressure drops are encountered during filling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³dry; ISO 1183
Water Absorption 0.90 %0.90 %24 hour; ISO Test
 5.7 %5.7 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 1.6 %1.6 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  38.0 MPa
@Temperature 120 °C
5510 psi
@Temperature 248 °F
ASTM Test
 38.0 MPa
@Temperature 120 °C
5510 psi
@Temperature 248 °F
ISO Data
 46.0 MPa
@Temperature 80.0 °C
6670 psi
@Temperature 176 °F
ISO Data
 46.0 MPa
@Temperature 80.0 °C
6670 psi
@Temperature 176 °F
ASTM Test
 153 MPa
@Temperature -40.0 °C
22200 psi
@Temperature -40.0 °F
ASTM Test
 153 MPa
@Temperature -40.0 °C
22200 psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Ultimate 67.0 MPa9720 psi5mm/min; ISO 527
Elongation at Break 5.6 %5.6 %5mm/min; ISO 527
 2.6 %
@Temperature -40.0 °C
2.6 %
@Temperature -40.0 °F
ISO Data
 2.6 %
@Temperature -40.0 °C
2.6 %
@Temperature -40.0 °F
ASTM Test
 5.9 %
@Temperature 80.0 °C
5.9 %
@Temperature 176 °F
ISO Data
 5.9 %
@Temperature 80.0 °C
5.9 %
@Temperature 176 °F
ASTM Test
 7.3 %
@Temperature 120 °C
7.3 %
@Temperature 248 °F
ASTM Test
 7.3 %
@Temperature 120 °C
7.3 %
@Temperature 248 °F
ISO Data
Tensile Modulus 3.90 GPa566 ksi1mm/min; ISO 527
 2.32 GPa
@Temperature 120 °C
336 ksi
@Temperature 248 °F
ISO Data
 3.05 GPa
@Temperature 80.0 °C
442 ksi
@Temperature 176 °F
ISO Data
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
 
Descriptive Properties
ColorBK-126
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned)
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Conditioned)
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)

PBASF9390 / 85154

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.