MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G HS BK-106. In parts containing cross sections, significant pressure drops are encountered during filling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccdry; ISO 1183
Water Absorption 0.90 %24 hour; ISO Test
 5.7 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 1.6 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.0040 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38.0 MPa
@Temperature 120 °C
ASTM Test
 38.0 MPa
@Temperature 120 °C
ISO Data
 46.0 MPa
@Temperature 80.0 °C
ISO Data
 46.0 MPa
@Temperature 80.0 °C
ASTM Test
 153 MPa
@Temperature -40.0 °C
ASTM Test
 153 MPa
@Temperature -40.0 °C
ISO Data
Tensile Strength, Ultimate 67.0 MPa5mm/min; ISO 527
Elongation at Break 5.6 %5mm/min; ISO 527
 2.6 %
@Temperature -40.0 °C
ISO Data
 2.6 %
@Temperature -40.0 °C
ASTM Test
 5.9 %
@Temperature 80.0 °C
ISO Data
 5.9 %
@Temperature 80.0 °C
ASTM Test
 7.3 %
@Temperature 120 °C
ASTM Test
 7.3 %
@Temperature 120 °C
ISO Data
Tensile Modulus 3900 MPa1mm/min; ISO 527
 2320 MPa
@Temperature 120 °C
ISO Data
 3050 MPa
@Temperature 80.0 °C
ISO Data
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10 K/min
 220 °CASTM Test
 
Descriptive Properties
ColorBK-126
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned)
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Conditioned)
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)

PBASF9390 / 85154

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.