Type: Estane® ALR CL600 is a Shore D thermoplastic polyurethane (TPU) resin. Features: Contains a UV package that enhances outdoor weatherability, but does not contain lubricants or wax processing aids. Uses: Outdoor applications Information Provided by The Lubrizol Corporation |