PlasGlas 50112 is a glass-filled polyester bulk molding that has been specially formulated to have the good heat-resistance, dimensional stability, and smooth surface required to function well as automotive halogen headlamp reflectors. It can be compression, transfer, or injection molded and is available in either bulk or extruded form. Data provided by Plaslok Corporation. Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products. |