MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polynt 30 CF60- 6mm Carbon Fiber VE BMC
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: Bulk molding compound based on Vinyl ester resin and reinforced with carbon fibers designed for compression molding technology. These materials with a potential weight reduced and a freedom high design enter different areas for structural application where high mechanical properties are requested.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183 A
Filler Content 60 %60 %Carbon
Linear Mold Shrinkage 0.00030 cm/cm0.00030 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psiISO 527-4
Tensile Modulus 19.0 GPa2760 ksiISO 527-4
Flexural Strength 110 MPa16000 psiISO 14125
Flexural Modulus 19.0 GPa2760 ksiISO 14125
Tensile Impact Strength 12.0 kJ/m²5.71 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Hold Pressure 3.00 - 8.998 MPa435 - 1305 psiMolding pressure
Cure Time 0.667 min
@Temperature 135 - 155 °C
0.0111 hour
@Temperature 275 - 311 °F
per mm
Shelf Life 2.00 Month
@Temperature 23.0 °C
2.00 Month
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polynt BMC 1150 Bulk Molding Compound ARC Ablation
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
Plenco PlasGlas™ 40118 High Strength Glass Filled Thermoset Polyester BMC
Polynt BMC 1151 GRIGIO Bulk Molding Compound ARC Ablation
Polynt BMC 580 Bulk Molding Compound Green Compound With Natural Fiber

PPOLYN9083 / 231678

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.