MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Asahi Kasei Thermylene® P-20TC-5103 20% Talc Reinforced, Lubricated, Heat Stabilized Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Information provided by Asahi Thermofil, now Asahi Kasei North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM D955
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength, Yield 31.0 MPa4500 psiASTM D638
Elongation at Yield 30 %30 %ASTM D638
Flexural Strength 48.3 MPa7000 psiASTM D790
Flexural Modulus 2.34 GPa340 ksiASTM D790
Izod Impact, Notched 0.347 J/cm0.650 ft-lb/inASTM D256
Izod Impact, Unnotched 6.41 J/cm12.0 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.4 µm/m-°C
@Temperature 20.0 °C
33.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 127 °C260 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C170 °FASTM D648
Flame Spread 20 mm/min0.80 in/minHorizontal Burn Rate; FMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Thermylene® P4-20TC-0520 PP-TD20FR
Asahi Kasei Thermylene® P-20TC-5100 20% Talc Filled, Heat Stabilized Polypropylene
Asahi Kasei Thermylene® P-20TC-0736 20% Talc Filled, Heat Stabilized Polypropylene
Asahi Kasei Thermylene® P-20FG-1740 20% Glass Fiber Reinforced, Medium Impact Polypropylene
Asahi Kasei Thermofil P-20TC-Y118 20% Talc Reinforced, Heat Stabilized Polypropylene

PTHER047 / 70146

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.