MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Thermylene® P4-20TC-0520 PP-TD20FR
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: 20% Talc Reinforcement with Flame Retardant (FR)

Information provided by Asahi Kasei North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183A
Melt Flow 6.0 g/10 min6.0 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 25.0 MPa3630 psiISO 527
Flexural Strength 41.0 MPa5950 psiISO 178
Flexural Modulus 2.90 GPa421 ksiISO 178
Charpy Impact, Notched 0.260 J/cm²1.24 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436C20L Calcium Reinforced
Overview of materials for Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 1-1120 AN 20% Talc-Filled Polypropylene Homopolymer
Aclo Accutech Polypropylene Homopolymer HP0336C20L1 Calcium Reinforced
Aclo Accutech Polypropylene Copolymer CP0436C20L1 Calcium Reinforced

PASAHI9904 / 220795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.