MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro Acclaim® 2220N Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Acclaim 2220N polyol is a 2,250-molecular-weight diol.

Properties / Applications: Acclaim 2220N polyol is a high-performance, low-monol polyether that is prepared with Covestro's proprietary IMPACT™ technology, using a patented organo-metallic propoxylation catalyst. The terminal end-groups have a high percentage of primary hydroxyl end-groups giving a relatively high reactivity with isocyanates. Because this product is not acidified, care must be taken using it in isocyanate- terminated prepolymers. Acclaim 2220N polyol is used in polyurethane and other urethane applications, including cast elastomers, sealants, adhesives, epoxy flexibilizers, defoamers, reaction injection molding (RIM), lubricants, crude oil de-emulsifiers, and plasticizers. This polyol contains extremely low levels of monol. In some polyurethane systems, formulation changes, such as reducing the cross-linking level or changing the hard-segment content, may be necessary to maximize the benefits of using Acclaim polyols. As with any product, the use of Acclaim 2220N polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
 0.960 g/cc
@Temperature 60.0 °C
0.960 g/cc
@Temperature 140 °F
 1.00 g/cc
@Temperature 20.0 °C
1.00 g/cc
@Temperature 68.0 °F
Bulk Density 1.03 g/cc0.0372 lb/in³
Viscosity 390 cP390 cP
 20 cP
@Temperature 80.0 °C
20 cP
@Temperature 176 °F
 100 cP
@Temperature 55.0 °C
100 cP
@Temperature 131 °F
Storage Temperature 15.0 - 60.0 °C59.0 - 140 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.015<= 0.015[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 218 °C424 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<150 Pt-Co
Hydroxyl number48.5-51.5 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmodur® BL 1100/1 Polyurethane
Covestro Acclaim® 2200 Polyol
Covestro Desmodur® BL 4265 SN Polyurethane
Covestro Desmodur 352 + Baytec 352P + Baytec XL B 76A Polyurethane, MDI Ester
Covestro Baytuft® 751A Polyurethane

PCOVEST0003 / 201786

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.