MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol STAT-RITE® X-5091 Ether-Type Static Dissipative Polymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Description: Inherently dissipative, this patented technology delivers surface resistivity in the range of 10E8 to 10E10 O/square. Stat-Rite® IDP Polymers forms a molecular-scale, interpenetrating polymer network which carries charge. The polymeric charge carriers are permanent over time even through customer processing in injection molding or extrusion. The fundamental Estane® TPU backbone dominates in property performance. Stat-Rite® IDP (Inherently Dissipative Polymer) is a homogeneous polymer which lends itself to consistent voltage decay throughout the matrix of a finished product. Conversely alternative technologies including the use of fillers or additives can off-gas, migrate, or slough-off causing contamination at a minimum and slow or inconsistent ESD protection. Stat-Rite® IDP Elastomer Alloys are based upon TPU providing the ultimate mechanical durability, low temperature flexibility and permanent ESD protection.

Major Benefits of Stat-Rite® IDP Elastomer Alloys:

  • Permanent static dissipation
  • Ultra-clean
  • Low off-gassing; low ionics
  • Clarity
  • No particulates
  • TPU performance

Applications:

  • Clean room soft walls, windows, and doors
  • Materials handling hose and tubing
  • Vacuum hose and tubing
  • Work surface mats

Specific Notes for this Material: Newer higher electrostatic dissipation (ESD) protection, permanent ESD without carbon or anti-stats

Information provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Tensile Strength, Ultimate 26.2 MPa3800 psiASTM D412/D638
Elongation at Break 450 %450 %ASTM D412/D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+9 ohm-cm5.00e+9 ohm-cmASTM D257
Surface Resistivity per Square 5.00e+9 ohm5.00e+9 ohmASTM D257

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy
Lubrizol Stat-Rite® M-809 Static Control Acrylic
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether

PNOVEON071 / 55336

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.