MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inASTM D995
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Hardness, Shore D 4242ASTM D2240
Tensile Strength at Break 50.0 MPa7250 psiDIN 53504
Elongation at Break 470 %470 %ASTM D412
100% Modulus 12.3 MPa
@Strain 100 %
1780 psi
@Strain 100 %
DIN 53504
300% Modulus 30.8 MPa
@Strain 300 %
4470 psi
@Strain 300 %
DIN 53504
Rebound 35 %35 %Bayshore; ASTM D2632
Tear Strength 105 kN/m600 pliASTM D624
Abrasion 3030[mm3]; ISO 4649
Compression Set  29 %
@Temperature 23.0 °C,
Time 252000 sec
29 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 82 %
@Temperature 70.0 °C,
Time 86400 sec
82 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 175 - 188 °C347 - 370 °FHuntsman/TMA
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not reported

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane

PHU9933 / 150393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.