MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Lupolen 3420J Low Density Polyethylene (LDPE), Blow Molding Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Lupolen 3420 J is a non-additivated, low density polyethylene. It is characterized by a good processability and high stiffness. LyondellBasell customers report that Lupolen 3420 J is used in label film and that films made from Lupolen 3420 J exhibit a glossy surface finish. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Food Packaging Film, Hygiene Film, Lamination Film, Surface Protection Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.934 g/cc0.0337 lb/in³ISO 1183-1
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 16.0 MPa2320 psiISO 527-1,-2
Film Elongation at Break, MD 500 %500 %ISO 527-1,-3
Film Elongation at Break, TD 650 %650 %ISO 527-1,-3
Tensile Modulus 0.480 GPa69.6 ksiISO 527-1,-2
Coefficient of Friction >= 0.65>= 0.65ISO 8295
Dart Drop Test 90.0 g0.198 lbF50; ASTM D 1709
Film Tensile Strength at Break, MD 22.0 MPa3190 psiISO 527-1,-3
Film Tensile Strength at Break, TD 20.0 MPa2900 psiISO 527-1,-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 119 °C246 °Fpeak; ISO 3146
Vicat Softening Point 109 °C228 °FA50N; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 10 %
@Thickness 0.0500 mm
<= 10 %
@Thickness 0.00197 in
ASTM D1003
Gloss >= 95 %>= 95 %@ 20°; ASTM D2457
 >= 115 %>= 115 %@ 60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 190 °C302 - 374 °FExtrusion Temperature
 
Descriptive Properties
Failure Energy (J/mm)3DIN 53373
Processing MethodBlown Film, Cast Film
Test Specimenfilm, 50µm blown film extruded at 170°C, and a blow up ratio 2.5:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT8551 / 220186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.