Lupolen 3420 J is a non-additivated, low density polyethylene. It is characterized by a good processability and high stiffness. LyondellBasell customers report that Lupolen 3420 J is used in label film and that films made from Lupolen 3420 J exhibit a glossy surface finish. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Food Packaging Film, Hygiene Film, Lamination Film, Surface Protection FilmInformation provided by LyondellBasell. |