Product Description: Lustran® 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applications, particularly in thin-walled components for telecommunications, office equipment, consumer and other office products. Features: Very high flow; Good impact strength; High gloss; UL 94 HB rated Applications: Telecommunications; Office equipment; Consumer and office productsAvailability: Latin America; North America Features: Good Impact Resistance; High Flow; High Gloss Uses: Business Equipment; Construction Applications; Telecommunications; Thin-walled Parts Processing Method: Injection Molding Information provided by INEOS Styrolution |