MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

INEOS Styrolution Lustran® 288 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: Lustran® 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applications, particularly in thin-walled components for telecommunications, office equipment, consumer and other office products.
Features: Very high flow; Good impact strength; High gloss; UL 94 HB rated
Applications: Telecommunications; Office equipment; Consumer and office products

Availability: Latin America; North America

Features: Good Impact Resistance; High Flow; High Gloss

Uses: Business Equipment; Construction Applications; Telecommunications; Thin-walled Parts

Processing Method: Injection Molding

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Water Absorption at Saturation 0.0095 %0.0095 %ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow  2.7 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.7 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 8.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 29 g/10 min
@Load 10.0 kg,
Temperature 200 °C
29 g/10 min
@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength, Yield 47.2 MPa6850 psiASTM D638
Elongation at Break 22 %22 %ASTM D638
Tensile Modulus 2.25 GPa326 ksiASTM D638
Flexural Yield Strength 65.4 MPa9490 psiASTM D790
Flexural Modulus 2.23 GPa324 ksiASTM D790
Izod Impact, Notched  0.854 J/cm
@Temperature -30.0 °C
1.60 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 2.24 J/cm
@Temperature 22.8 °C
4.20 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.7 °C197 °FUnannealed
 98.9 °C210 °FAnnealed
Deflection Temperature at 1.8 MPa (264 psi) 83.3 °C182 °FUnannealed
 96.1 °C205 °FAnnealed
 
Optical PropertiesMetricEnglishComments
Gloss 79 %79 %60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Mold Temperature 43.3 - 65.6 °C110 - 150 °F
Drying Temperature 79.4 °C175 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTYS766 / 311459

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.