MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Petromont 1002 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion blow moulding machines to produce containers up to 10 litres for use in various packaging applications. The glossy appearance that is characteristic of Pétromont`s resins results in parts with good surface quality.

Combining its low melt index and high density, Petromont HDPE 1002 exhibits excellent rigidity and top load performance while maintaining outstanding drop impact properties and excellent environmental stress cracking properties. The specially designed formulation makes Petromont HDPE 1002 less susceptible to degradation during processing. This product is also Anti-static modified.

Key Words: Pharmaceutical grade, with antistat
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D1505
ESCR 100% Igepal® 33 hourF50; ASTM D1693-B
Melt Flow 0.33 g/10 minI2; ASTM D1238
 29 g/10 minI21; ASTM D238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D2240
Tensile Strength, Yield 26.9 MPaASTM D638
Elongation at Break >= 800 %ASTM D638
Flexural Modulus 1.325 GPaASTM D790
Izod Impact, Notched 160 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 134 °CPetromont
Crystallization Temperature 111 °CPetromont
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °CASTM D648
Vicat Softening Point 128 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746
 
Descriptive Properties
ProcessBlow Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Petromont 1000 High Density Polyethylene Resin
DuPont 20 Series 2020T Specialty Polyethylene Resin
Dow ELITE™ 5401G Enhanced Polyethylene Resin
Dow DOWLEX™ 2085G Polyethylene Resin
Total 3720Z Polypropylene, Injection Molding Grade

PPETROM01 / 56195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.