MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petromont 1000 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to produce containers up to 10 litres for use in various packaging applications. Petromont HDPE 1000 offers both excellent processing characteristics and finish product performance.

Petromont HDPE 1000, because of its high density, exhibits excellent rigidity and top load performance while still offering outstanding drop impact properties, as well as maintaining excellent environmental stress crack resistance performance. The higher density also makes this product a good candidate for some hot filled applications. The glossy appearance, which is characteristic of Pétromont’s resins, results in parts exhibiting good surface quality. The highly stabilized additive package makes Petromont HDPE 1000 less susceptible to degradation during processing. In regards to swell characteristics, Petromont HDPE 1000 is similar to most competitive resins having similar viscosity properties.

Key Words: Pharmaceutical grade, containers, packaging
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ASTM D1505
ESCR 100% Igepal® 33 hour33 hourF50; ASTM D1693-B
Melt Flow 0.33 g/10 min0.33 g/10 minI2; ASTM D1238
 29 g/10 min29 g/10 minI21; ASTM D238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ASTM D2240
Tensile Strength, Yield 26.9 MPa3900 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus 1.325 GPa192.2 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature 20.0 °C
72.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 134 °C273 °FPetromont
Crystallization Temperature 111 °C232 °FPetromont
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °FASTM D648
Vicat Softening Point 128 °C262 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Descriptive Properties
ProcessBlow Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos T50-500 HDPE
Petromont 1002 High Density Polyethylene Resin
Isoflon PEHD 1000 High Density Polyethylene
Borealis Bormed™ DM55pharm Polypropylene
DuPont 20 Series 2020T Specialty Polyethylene Resin

PPETROM00 / 56194

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.