MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
J6 Polymers JFOAM™ BX-650 Engineered Specialty Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: JFoam™ BX-650 is a two component rigid polyurethane foam system designed for structural void filling applications. This system is well suited for RTM applications where high compressive and tensile strength properties are required during post curing of composite part. BX-650 has a recommended service temperature of 225°F.

Information provided by J6 Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.094 g/cc
Density 6.20 lb/ft³Free Rise, #10 cup
 10.0 - 12.0 lb/ft³Molded, overall
 11.3 lb/ft³Core
Viscosity 200 cPT Component, Polymeric MDI
 1600 cPR Component, Polyol Blend
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 42.0 psiASTM C273
Compressive Strength 120 psi
@Temperature 177 °C
Perpendicular; ASTM D1621
 340 psi
@Temperature 25.0 °C
Parallel; ASTM D1621
Compressive Modulus 2870 psi
@Temperature 177 °C
ASTM D1621
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 225 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Hand Mix Reactivity155 secSting Time
 80 secCream Time
Mixing Ratio0.35R Component, Polyol Blend
 0.65T Component, Polymeric MDI

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSIX012 / 190939

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.